IP Library Granted Patent US 12,676,344
Granted Patent B2
US 12,676,344 · App. 18/443,169 · Granted Jul 7, 2026

Electrochemical cells and methods of manufacturing thereof

Inventors: Pietro Papa Lopes (Woodridge, IL); Timothy Fister (Oak Park, IL); Susan J. Babinec (Midland, MI); Vojislav Stamenkovic (Naperville, IL)
Assignee: UCHICAGO ARGONNE, LLC
H01M10/4242H01M10/128H01M10/44
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 12,676,344
App. No.
18/443,169
Filed
Feb 15, 2024
Granted
Jul 7, 2026
Kind
B2
Art Unit
1724
USPC
429/49
Abstract

An electrochemical cell includes a housing, a positive electrode substrate disposed within a first electrode chamber of the housing, a negative electrode substrate disposed within a second electrode chamber of the housing, and a separator may be disposed within the housing between the first electrode chamber and the second electrode chamber. A method further includes pumping a manufacturing electrolyte through the positive electrode portion around the positive electrode substrate. The method further includes applying a first electrical signal to the positive electrode substrate so as to electrochemically fabricate one or both of an active material the negative electrode substrate to form a negative electrode and/or an active material on the positive electrode substrate, thereby forming a positive electrode.

Claims (45)

1 . A method, comprising;

passing a first manufacturing electrolyte and a second manufacturing electrolyte through an electrochemical cell simultaneously by:

pumping the first manufacturing electrolyte through a first electrode chamber around a negative electrode substrate of the electrochemical cell;

pumping the second manufacturing electrolyte through a second electrode chamber around a positive electrode substrate of the electrochemical cell; and

applying a first electrical signal to the electrochemical cell to electrochemically fabricate a negative active material on the negative electrode substrate, and to electrochemically fabricate a positive active material on the positive electrode substrate.

2 . The method of claim 1 , wherein at least one of the negative active material and the positive active material comprises Pb, PbO 2 , or a combination thereof.

3 . The method of claim 1 , further comprising, after formation of the negative active material and the positive active material, pumping a charge operation electrolyte through the electrochemical cell while applying a second electrical signal to the electrochemical cell to charge the electrochemical cell.

4 . The method of claim 3 , further comprising, after pumping the charge operation electrolyte:

switching the electrochemical cell to an open circuit voltage; and

flowing from a reservoir an open circuit electrolyte through the electrochemical cell, the open circuit electrolyte having a concentration providing a non-equilibrium steady state in the electrochemical cell, thereby dispensing the charge operation electrolyte out of the electrochemical cell.

5 . The method of claim 3 , further comprising, after pumping the charge operation electrolyte, pumping a first regeneration electrolyte through the first electrode chamber around the negative electrode substrate of the electrochemical cell and pumping a second regeneration electrolyte through the second electrode chamber around the positive electrode substrate of the electrochemical cell, wherein the first regeneration electrolyte is configured to remove spent active material from the negative electrode substrate and the second regeneration electrolyte is configured to remove spent active material from the positive electrode substrate.

6 . The method of claim 5 , wherein the first regeneration electrolyte comprises:

water in a concentration of about 0.01 vol % to about 99.999 vol %;

an alkaline solution or an acid in a concentration of about 0.01 vol % to about 99.999 vol %; and

wherein the acid comprises sulfuric acid, nitric acid, methane sulfonic acid, or a combination of two or more thereof.

7 . The method of claim 6 , wherein the second regeneration electrolyte comprises:

water in a concentration of about 0.01 vol % to about 99.999 vol %;

an alkaline solution or an acid in a concentration of about 0.01 vol % to about 99.999 vol %; and

wherein the acid comprises sulfuric acid, nitric acid, methane sulfonic acid, or a combination of two or more thereof.

8 . The method of claim 5 , further comprising, after removal of the spent active material,

pumping the first manufacturing electrolyte through the first electrode chamber around the negative electrode substrate;

pumping the second manufacturing electrolyte through the second electrode chamber around the positive electrode substrate; and

applying the first electrical signal to the electrochemical cell to electrochemically refabricate the negative active material on the negative electrode substrate, and to electrochemically refabricate the positive active material on the positive electrode substrate.

9 . The method of claim 1 , wherein at least one of the first manufacturing electrolyte or the second manufacturing electrolyte comprises one or more of sulfuric acid, nitric acid, or methane sulfonic acid in a concentration in a range of 0.01% to 99.99%.

10 . The method of claim 1 , wherein at least one of the first manufacturing electrolyte or the second manufacturing electrolyte comprises lead ions in a concentration in a range of 0.01 mM to 1 M.

11 . The method of claim 1 , wherein pumping the first manufacturing electrolyte through the first electrode chamber comprises flowing the first manufacturing electrolyte through the first electrode chamber at a rate of 0.001 liters/minute/cm 2 to 100 liters/minute/cm 2 .

12 . The method of claim 1 , wherein pumping the second manufacturing electrolyte through the second electrode chamber comprises flowing the second manufacturing electrolyte through the second electrode chamber at a rate of 0.001 liters/minute/cm 2 to 100 liters/minute/cm 2 .

13 . An electrochemical cell assembly comprising:

an electrochemical cell comprising a negative electrode substrate;

a first electrolyte reservoir fluidically coupled with the electrochemical cell, the first electrolyte reservoir comprising a first manufacturing electrolyte to electrochemically formulate active material on the negative electrode substrate, forming a negative electrode;

a second electrolyte reservoir fluidically coupled with the electrochemical cell, the second electrolyte reservoir comprising a charge operation electrolyte to facilitate reduction at the negative electrode during charging of the electrochemical cell; and

a third electrolyte reservoir fluidically coupled with the electrochemical cell, the third electrolyte reservoir comprising a discharge operation electrolyte to facilitate oxidation at the negative electrode during discharging of the electrochemical cell.

14 . The electrochemical cell assembly of claim 13 , wherein the electrochemical cell comprises:

the negative electrode substrate disposed within a first electrode chamber; and

a positive electrode substrate disposed within a second electrode chamber.

15 . The electrochemical cell assembly of claim 14 , further comprising a fourth electrolyte reservoir fluidically coupled with the electrochemical cell, the fourth electrolyte reservoir comprising a second manufacturing electrolyte,

wherein the second manufacturing electrolyte is formulated to electrochemically fabricate an active material on the positive electrode substrate.

16 . The electrochemical cell assembly of claim 15 , further comprising a pump assembly configured to pump the first manufacturing electrolyte through the first electrode chamber and pump the second manufacturing electrolyte through the second electrode chamber.

17 . The electrochemical cell assembly of claim 15 , further comprising a fifth electrolyte reservoir fluidically coupled with the electrochemical cell, the fifth electrolyte reservoir comprising a regeneration electrolyte configured to remove a spent active material from one or both of the positive electrode substrate and the negative electrode substrate.

18 . The electrochemical cell assembly of claim 17 , wherein the regeneration electrolyte comprises:

water in a concentration of about 0.01 vol % to about 99.999 vol %;

an alkaline solution or an acid in a concentration of about 0.01 vol % to about 99.999 vol %; and

wherein the acid comprises sulfuric acid, nitric acid, methane sulfonic acid, or a combination of two or more thereof.

19 . The electrochemical cell assembly of claim 15 , wherein at least one of the first manufacturing electrolyte or the second manufacturing electrolyte comprises lead ions in a concentration in a range of 0.01 mM to 1 M.

20 . The electrochemical cell assembly of claim 15 , wherein at least one of the first manufacturing electrolyte or the second manufacturing electrolyte comprises acid in a concentration of about 0.01 vol % to about 99.999 vol %.

Assignments (2)
CONFIRMATORY LICENSE Recorded May 3, 2024
From: UCHICAGO ARGONNE LLC
To: U.S. DEPARTMENT OF ENERGY
Reel/Frame 067310/0611 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Mar 11, 2024
From: LOPES, PIETRO PAPA; FISTER, TIMOTHY; BABINEC, SUSAN J.; STAMENKOVIC, VOJISLAV
To: UCHICAGO ARGONNE, LLC
Reel/Frame 066718/0378 →
Continuity (2)
Continuation 17587644 · Jan 28, 2022
Related Publication 20240186592A1 · Jun 6, 2024
References Cited (38)
US 3915745A · Ikeda et al. · 1975 [cited by applicant]
US 5612148A · Zito · 1997 [cited by applicant]
US 5650239A · Lex et al. · 1997 [cited by applicant]
US 8048555B2 · Darcy et al. · 2011 [cited by applicant]
US 9722236B2 · Sathrum · 2017 [cited by applicant]
US 10615441B2 · Kaku · 2020 [cited by examiner]
US 20040151977A1 · Morrisey et al. · 2004 [cited by applicant]
US 20060063065A1 · Clarke et al. · 2006 [cited by applicant]
US 20070111043A1 · Stocchiero · 2007 [cited by applicant]
US 20100003545A1 · Horne et al. · 2010 [cited by applicant]
US 20100036450A1 · Axelrod et al. · 2010 [cited by applicant]
US 20120135282A1 · La Mantia et al. · 2012 [cited by applicant]
US 20130011702A1 · Horne et al. · 2013 [cited by applicant]
US 20130084506A1 · Chang et al. · 2013 [cited by applicant]
US 20140060666A1 · Evans · 2014 [cited by examiner]
US 20140220463A1 · Daniel · 2014 [cited by applicant]
US 20140266058A1 · Sathrum · 2014 [cited by applicant]
US 20150086896A1 · Chang et al. · 2015 [cited by applicant]
US 20150099206A1 · Horne et al. · 2015 [cited by applicant]
US 20150318580A1 · Fukunaga et al. · 2015 [cited by applicant]
US 20160020477A1 · Smeltz et al. · 2016 [cited by applicant]
US 20160293992A1 · Song et al. · 2016 [cited by applicant]
US 20170271705A1 · Kim et al. · 2017 [cited by applicant]
US 20180198148A1 · Pozvonkov et al. · 2018 [cited by applicant]
US 20190237792A1 · Ikeuchi · 2019 [cited by applicant]
US 20190280316A1 · Min · 2019 [cited by examiner]
US 20200076017A1 · Shen et al. · 2020 [cited by applicant]
US 20200106118A1 · Wang et al. · 2020 [cited by applicant]
US 20210143463A1 · Song et al. · 2021 [cited by applicant]
US 20210143488A1 · Kong et al. · 2021 [cited by applicant]
US 20230144710A1 · Saraidaridis et al. · 2023 [cited by applicant]
CN 105845960A · 2016 [cited by applicant]
Collins, et al., “A novel flow battery: A lead acid battery based on an electrolyte with soluble lead(II) Part VIII. The cycling of a 10 cm x 10 cm flow cell,” Journal of Power Sources 195(6), pp. 1731-1738 (2010). [cited by applicant]
Consortium for Battery Innovation, “An innovation roadmap for advanced lead batteries: Technical specifications and performance improvements,” retrieved from https://batteryinnovation.org/wp-content/uploads/2019/09/CBIR… [cited by applicant]
Hazza, et al., “A novel flow battery—A lead acid battery based on an electrolyte with soluble lead(II): IV. The influence of additives,” Journal of Power Sources 149, pp. 103-111 (2005). [cited by applicant]
International Search Report & Written Opinion on PCT/US2022/053872 dated Apr. 12, 2023, 10 pages. [cited by applicant]
International Search Report & Written Opinion on PCT/US2022/053880 dated Apr. 12, 2023, 7 pages. [cited by applicant]
Pletcher & Wills, “A novel flow battery—A lead acid battery based on an electrolyte with soluble lead(II): III. The influence of conditions on battery performance,” Journal of Power Sources 149, pp. 96-102 (2005). [cited by applicant]