IP Library Granted Patent US 9,287,317
Granted Patent B2
US 9,287,317 · App. 14/154,758 · Granted Mar 15, 2016

Image sensor module and method of manufacturing the same

Inventors: Ji Bum Cha (Gyunggi-do, KR); Sung Jae Lee (Gyunggi-do, KR); In Cheol Chang (Gyunggi-do, KR); Sung Jun Byun (Gyunggi-do, KR)
Assignee: Samsung Electro-Mechanics Co., Ltd.
H01L27/14685H01L24/83H01L27/14618H01L27/14625H01L27/14683H04N5/2257H01L2224/83192H01L2224/83856H01L2924/3511
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,287,317
App. No.
14/154,758
Granted
Mar 15, 2016
Kind
B2
Abstract

There is provided an image sensor module, including: an image sensor having a small thickness of 175 μm or less and having a first coefficient of thermal expansion; a substrate having the image sensor mounted thereon and having a second coefficient of thermal expansion higher than the first coefficient of thermal expansion; and an adhesive layer disposed between the image sensor and the substrate and including an adhesive having a third coefficient of thermal expansion of 130 ppm/° C. or more at a glass transition temperature Tg or more.

Claims (9)

1. A method of manufacturing an image sensor module for a subminiature camera, the method comprising:

dispensing an adhesive having a third coefficient of thermal expansion of 130 ppm/° C. or more at a glass transition temperature Tg or more of the adhesive to a substrate having a second coefficient of thermal expansion and a thickness of 175 μm or less, the adhesive having a thickness less than that of the image sensor;

temporarily curing and attaching an image sensor having a first coefficient of thermal expansion to the substrate to which the adhesive has been dispensed; and

curing the adhesive at the glass transition temperature Tg or more of the adhesive, the glass transition temperature of the adhesive being lower than a curing temperature of the adhesive,

wherein pressure is applied for 1 to 2 seconds at a temperature range of 120° C. to 160° C. in the attaching of the image sensor to the substrate, and

the curing of the adhesive is performed for about 120 seconds at about 120° C.

2. The method of claim 1 , wherein the adhesive is applied to form an adhesive layer thinner than the image sensor.

3. The method of claim 1 , wherein the substrate includes a copper clad laminate (CCL).

4. The method of claim 1 , wherein the adhesive includes an epoxy-based adhesive.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jan 14, 2014
From: CHA, JI BUM; LEE, SUNG JAE; CHANG, IN CHEOL; BYUN, SUNG JUN
To: SAMSUNG ELECTRO-MECHANICS CO., LTD.
Reel/Frame 031964/0646 →
Priority Claims (1)
KR 10-2013-0154119 · Dec 11, 2013 · national
Continuity (2)
Provisional Application 61756802 · Jan 25, 2013
Related Publication 20140210027A1 · Jul 31, 2014