Decomposable S-tetrazine based polymers for single walled carbon nanotube applications

Inventors: Zhao Li (Orleans, CA); Jianfu Ding (Orleans, CA); Patrick Roland Lucien Malenfant (Orleans, CA)
Assignee: National Research Council of Canada
G01N27/4141C01B32/159G01N27/4146H01L51/0048H01L51/0545C01B2202/02H01L51/0002H01L51/0003H01L51/0026H01L51/0558
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,222,346
App. No.
15/708,855
Granted
Mar 5, 2019
Kind
B2
Abstract

A process for purifying semiconducting single-walled carbon nanotubes (sc-SWCNTs) extracted with a conjugated polymer, the process comprising exchanging the conjugated polymer with an s-tetrazine based polymer in a processed sc-SWCNT dispersion that comprises the conjugated polymer associated with the sc-SWCNTs. The process can be used for production of thin film transistors and chemical sensors. In addition, disclosed herein is use of an s-tetrazine based polymer for purification of semiconducting single-walled carbon nanotubes (sc-SWCNTs).

Claims (13)

1. A process for producing a chemical sensor that detects one or more chemicals in the ppt to ppb range, the process comprising:

a) applying a dispersion of a sc-SWCNT/s-tetrazine based conjugated polymer composite to a substrate;

b) applying heat and/or UV light to decompose the s-tetrazine based conjugated polymer; and

c) removing the resulting decomposition products.

2. The process of claim 1 , wherein the sensor has a lower detection limit of from 4 ppt to 100 ppb.

3. The process of claim 1 , wherein the one or more chemicals is gaseous ammonia or gaseous nitrogen dioxide (NO 2 ).

4. The process of claim 1 , wherein the s-tetrazine based polymer has the following structure:

where A is O, S, Se or C═C; n is an integer from 1 to 4; R 1 is independently H, F, CN or a C1-C20 linear or branched aliphatic group; Ar is one or more substituted or unsubstituted aromatic units; and, m is an integer 5 or greater.

5. The process of claim 1 , wherein the s-tetrazine based polymer is PBDTFTz:

6. The process of claim 1 , wherein the s-tetrazine based polymer is PDTSTTz:

7. The process of claim 1 , wherein the s-tetrazine based polymer is PCPDTFTz:

in which Ar=cyclopenta[2,1-b;3.4-b′]dithiophene.

8. The process of claim 1 , wherein the conjugated polymer comprises a polyfluorene or polythiophene.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Aug 14, 2018
From: LI, ZHAO; DING, JIANFU; MALENFANT, PATRICK ROLAND LUCIEN
To: NATIONAL RESEARCH COUNCIL OF CANADA
Reel/Frame 046791/0232 →
Continuity (2)
Continuation In Part 15401421 · Jan 9, 2017
Related Publication 20180195997A1 · Jul 12, 2018