IP Library Granted Patent US 10,876,384
Granted Patent B2
US 10,876,384 · App. 16/434,287 · Granted Dec 29, 2020

Methods of utilizing carbon monoxide to increase oil recovery and protect tubulars

Inventor: Paul B. Trost (Golden, CO)
E21B43/168C01B32/40C09K8/594C09K8/70E21B43/164E21B43/26C09K8/52C09K2208/32
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,876,384
App. No.
16/434,287
Granted
Dec 29, 2020
Kind
B2
Abstract

A method of utilizing carbon monoxide to increase oil recovery includes injecting an effective amount of carbon monoxide, either as pure carbon monoxide or as a component of a gas mixture, into an oil reservoir. The carbon monoxide increases oil flow and rate of oil flow from the oil reservoir through a variety of chemical mechanisms. The carbon monoxide also reduces corrosion in oilfield tubulars due to the formation of a reduced iron species coating on previously oxidized (corroded) areas.

Claims (8)

1. A method of protecting oilfield tubulars from corrosion, the method including injecting a gas mixture comprising carbon dioxide and at least 10% carbon monoxide into a reservoir at a natural unheated temperature in the range of 50° F. to 250° F. having tubulars therein, and reacting the carbon monoxide with an oxidized iron species on the oilfield tubulars to reduce the oxidized iron species on the oilfield tubulars.

2. The method of protecting oilfield tubulars from corrosion according to claim 1 , wherein the gas mixture comprises at least 20% carbon monoxide.

3. The method of protecting oilfield tubulars from corrosion according to claim 1 , wherein the gas mixture comprises at least 30% carbon monoxide.

4. The method of protecting oilfield tubulars from corrosion according to claim 1 , wherein the gas mixture comprises at least 40% carbon monoxide.

5. The method of protecting oilfield tubulars from corrosion according to claim 1 , wherein the gas mixture comprises the carbon monoxide and at least one of nitrogen (N 2 ), methane (CH 4 ), ethane (C 2 H 6 ), propane (C 3 H 8 ), butane (C 4 H 10 ) or pentane (C 5 H 12 ).

6. The method of protecting oilfield tubulars from corrosion according to claim 1 , wherein the carbon monoxide reacts with the oxidized iron species on the oilfield tubulars to produce FeO.

7. The method of protecting oilfield tubulars from corrosion according to claim 1 , wherein the carbon monoxide reacts with and reduces ferric oxides and hydroxides on the oilfield tubulars to reduced ferrous compounds.

8. The method of protecting oilfield tubulars from corrosion according to claim 7 , wherein the carbon monoxide reacts with and reduces the ferric oxides and hydroxides to FeO.

Continuity (6)
Division 15918883 · Mar 12, 2018
Continuation In Part 14621531 · Feb 13, 2015
Continuation In Part 13935925 · Jul 5, 2013
Continuation In Part 13438820 · Apr 3, 2012
Provisional Application 61940018 · Feb 14, 2014
Related Publication 20190284916A1 · Sep 19, 2019
Cited By (1)
US 12,460,523