IP Library › Granted Patent US 11,211,285
Granted Patent B2
US 11,211,285 · App. 16/962,311 · Granted Dec 28, 2021

Method of producing bonded wafer and bonded wafer

Inventors: Youzou Satou (Tokyo, JP); Kazuaki Kozasa (Tokyo, JP)
Assignee: SUMCO CORPORATION
H01L21/76251H01L29/0649
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 11,211,285
App. No.
16/962,311
Granted
Dec 28, 2021
Kind
B2
Abstract

In a method of producing a bonded wafer, the amount of depression of the polishing cloth is 50 μm to 90 μm, and the surface hardness (ASKER C) of the polishing cloth is 50 to 60. In the bonded wafer, the polycrystalline silicon layer has a thickness variation Δt of 5% or less, and the support substrate wafer has a GBIR of 0.2 μm or less and an SFQR of 0.06 μm or less after the polycrystalline silicon layer is polished.

Claims (13)

1. A method of producing a bonded wafer by bonding a support substrate wafer and an active layer wafer with an insulating film therebetween, comprising:

a polycrystalline silicon deposition step of depositing a polycrystalline silicon layer on the support substrate wafer on the bonding surface side;

a polycrystalline silicon layer polishing step of polishing a surface of the polycrystalline silicon layer using a polishing cloth:

an insulating film formation step of forming the insulating film on at least one of a bonding surface of the support substrate wafer and a bonding surface of the active layer wafer; and

a bonding step of bonding the polished surface of the polycrystalline silicon layer of the support substrate wafer and the active layer wafer with the insulating film therebetween,

wherein when an amount of depression of the polishing cloth is defined as:

Amount of depression (μm)=Thickness of polishing cloth (μm)×Compression ratio (%/(N/cm 2 ))×Load (N/cm 2 ),

the amount of depression of the polishing cloth is 50 μm to 90 μm, and a surface hardness (ASKER C) of the polishing cloth is 50 to 60.

2. The method of producing a bonded wafer, according to claim 1 , wherein the polishing cloth is a suede pad composed of a base and a nap layer.

3. The method of producing a bonded wafer, according to claim 2 , wherein the thickness of the base is 0.15 mm to 0.20 mm.

4. A bonded wafer comprising a polycrystalline silicon layer deposited on a support substrate wafer,

wherein the polycrystalline silicon layer has a thickness variation Δt of 5% or less, and

the support substrate wafer has a GBIR of 0.2 μm or less and an SFQR of 0.06 μm or less after the polycrystalline silicon layer is polished.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jul 15, 2020
From: SATOU, YOUZOU; KOZASA, KAZUAKI
To: SUMCO CORPORATION
Reel/Frame 053216/0831 →
Priority Claims (1)
JP JP2018-005914 · Jan 17, 2018 · national
Continuity (1)
Related Publication 20200343130A1 · Oct 29, 2020