Single-layer and multilayer graphene, method of manufacturing the same, object including the same, and electric device including the same

Inventors: Teppei Oguni (Kanagawa, JP); Takeshi Osada (Kanagawa, JP); Toshihiko Takeuchi (Kanagawa, JP); Kuniharu Nomoto (Saitama, JP)
Assignee: SEMICONDUCTOR ENERGY LABORATORY CO., LTD.
H01M4/587B82Y30/00B82Y40/00C25D5/48C25D5/50C25D13/02C25D13/12H01M4/0452H01M4/0471H01M4/133H01M4/1393H01M4/66H01M4/70Y02E60/10Y10T428/24355
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 11,296,322
App. No.
16/862,651
Granted
Apr 5, 2022
Kind
B2
Abstract

Graphene is formed with a practically uniform thickness on an uneven object. The object is immersed in a graphene oxide solution, and then taken out of the solution and dried; alternatively, the object and an electrode are immersed therein and voltage is applied between the electrode and the object used as an anode. Graphene oxide is negatively charged, and thus is drawn to and deposited on a surface of the object, with a practically uniform thickness. After that, the object is heated in vacuum or a reducing atmosphere, so that the graphene oxide is reduced to be graphene. In this manner, a graphene layer with a practically uniform thickness can be formed even on a surface of the uneven object.

Claims (59)

1. An electrode comprising:

a current collector;

an active material layer over the current collector, the active material layer having an uneven surface comprising projections and depressions; and

a plurality of graphene layers over the uneven surface,

wherein the active material layer comprises silicon,

wherein a first part of the plurality of graphene layers is in contact with the uneven surface,

wherein a space is formed between a second part of the plurality of graphene layers and one of the depressions of the uneven surface,

wherein a number of layers of the plurality of graphene layers is 50 or less,

wherein each of the plurality of graphene layers has at least one pore, and

wherein the pore of a first layer of the plurality of graphene layers does not overlap the pore of a second layer adjacent to the first layer of the plurality of graphene layers.

2. The electrode according to claim 1 ,

wherein the uneven surface comprises a plurality of silicon whiskers.

3. The electrode according to claim 2 ,

wherein the plurality of silicon whiskers comprise a first whisker and a second whisker; and

wherein the first part of the plurality of graphene layers connects the first whisker to the second whisker.

4. The electrode according to claim 1 ,

wherein a thickness of the plurality of graphene layers over the uneven surface is substantially uniform.

5. The electrode according to claim 1 ,

wherein a concentration of elements other than carbon and hydrogen contained in the plurality of graphene layers is lower than or equal to 15 atomic %, and

wherein a concentration of oxygen contained in the plurality of graphene layers is higher than or equal to 5 atomic % and lower than or equal to 15 atomic %.

6. A lithium-ion secondary battery comprising the electrode according to claim 1 , wherein the electrode is used as an electrode of the lithium-ion secondary battery.

7. An electrode comprising:

a current collector;

an active material layer over the current collector, the active material layer having an uneven surface comprising projections and depressions; and

a plurality of graphene layers over the uneven surface,

wherein the active material layer comprises silicon,

wherein a part of the plurality of graphene layers is in contact with the uneven surface,

wherein a number of layers of the plurality of graphene layers is 50 or less,

wherein each of the plurality of graphene layers has at least one pore, and

wherein the pore of a first layer of the plurality of graphene layers does not overlap the pore of a second layer adjacent to the first layer of the plurality of graphene layers.

8. The electrode according to claim 7 ,

wherein the uneven surface comprises a plurality of silicon whiskers.

9. The electrode according to claim 8 ,

wherein the plurality of silicon whiskers comprise a first whisker and a second whisker; and

wherein the part of the plurality of graphene layers connects the first whisker to the second whisker.

10. The electrode according to claim 7 ,

wherein the number of layers of the plurality of graphene layers over the uneven surface is substantially uniform.

11. The electrode according to claim 7 ,

wherein a concentration of elements other than carbon and hydrogen contained in the plurality of graphene layers is lower than or equal to 15 atomic %, and

wherein a concentration of oxygen contained in the plurality of graphene layers is higher than or equal to 5 atomic % and lower than or equal to 15 atomic %.

12. A lithium-ion secondary battery comprising the electrode according to claim 7 , wherein the electrode is used as an electrode of the lithium-ion secondary battery.

13. An electrode comprising:

a current collector;

an active material layer over the current collector, the active material layer having an uneven surface; and

a plurality of graphene layers over the uneven surface,

wherein the active material layer comprises silicon,

wherein a number of layers of the plurality of graphene layers is 20 or less,

wherein each of the plurality of graphene layers has at least one pore, and

wherein the pore of a first layer of the plurality of graphene layers does not overlap the pore of a second layer adjacent to the first layer of the plurality of graphene layers.

14. The electrode according to claim 13 ,

wherein the uneven surface comprises a plurality of silicon whiskers.

15. The electrode according to claim 14 ,

wherein the plurality of silicon whiskers comprise a first whisker and a second whisker; and

wherein a part of the plurality of graphene layers connects the first whisker to the second whisker.

16. The electrode according to claim 13 ,

wherein the number of layers of the plurality of graphene layers over the uneven surface is substantially uniform.

17. The electrode according to claim 13 ,

wherein a thickness of the plurality of graphene layers over the uneven surface is substantially uniform.

18. A lithium-ion secondary battery comprising the electrode according to claim 13 , wherein the electrode is used as an electrode of the lithium-ion secondary battery.

Priority Claims (2)
JP 2011-124952 · Jun 3, 2011 · national
JP 2011-125027 · Jun 3, 2011 · national
Continuity (2)
Continuation 13483297 · May 30, 2012
Related Publication 20200259179A1 · Aug 13, 2020
Cited By (1)