IP Library › Granted Patent US 12,331,462
Granted Patent B2
US 12,331,462 · App. 17/791,862 · Granted Jun 17, 2025

Method for manufacturing bleached pulp from a feedstock comprising recycled paper

Inventors: Peter W. Hart (Atlanta, GA); John D. Dejarnette (Henrico, VA); Fritz G. Paulsen (Summerville, SC); Ashok K. Ghosh (Henrico, VA)
Assignee: WestRock MWV, LLC
D21C5/022D21B1/061D21C1/10D21C3/02D21C7/00D21C9/02D21C9/10D21H11/14
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 12,331,462
App. No.
17/791,862
Granted
Jun 17, 2025
Kind
B2
Abstract

A method for manufacturing bleached pulp from a feedstock that includes recycled paper. The method includes steps of: (1) impregnating the feedstock with cooking liquor to yield an impregnated material having a liquor-to-fiber mass ratio of at most about 4:1; (2) cooking the impregnated material to remove at least a portion of the lignin within the impregnated material, thereby yielding a cooked pulp; and (3) bleaching the cooked pulp.

Claims (37)

1. A method for manufacturing bleached pulp from a feedstock comprising recycled paper, the recycled paper comprising lignin and cellulose, the method comprising:

impregnating the feedstock with cooking liquor to yield an impregnated material having a liquor-to-fiber mass ratio of at most about 4:1, wherein the impregnating the feedstock comprises compressing the feedstock, wherein the compressing the feedstock achieves a compression ratio greater than 1:1, on a volume basis;

determining a cooking liquor uptake of the feedstock at the compression ratio achieved during the impregnating; and

tuning a charge of the cooking liquor added to the feedstock during the impregnating based on the cooking liquor uptake of the feedstock and a concentration of the cooking liquor;

cooking the impregnated material to remove at least a portion of the lignin from the impregnated material, thereby yielding a cooked pulp; and

bleaching the cooked pulp.

2. A method for manufacturing bleached pulp, the method comprising:

providing a feedstock comprising recycled paper, the recycled paper comprising lignin and cellulose, wherein the feedstock has a solids content of at least 70 percent by weight;

compressing the feedstock having the solids content of at least 70 percent by weight, thereby yielding a compressed feedstock;

impregnating the compressed feedstock with cooking liquor to yield an impregnated material having a liquor-to-fiber mass ratio of at most about 4:1;

feeding the impregnated material having the liquor-to-fiber mass ratio of at most about 4:1 to a digester;

cooking the impregnated material having the liquor-to-fiber mass ratio of at most about 4:1 to remove at least a portion of the lignin from the impregnated material, thereby yielding a cooked pulp; and

bleaching the cooked pulp.

3. The method of claim 2 wherein the feedstock has a solids content of at least 75 percent by weight.

4. The method of claim 2 wherein the feedstock has a kappa number of at least about 80.

5. The method of claim 2 wherein the feedstock comprises old corrugated containers.

6. The method of claim 2 wherein the compressing the feedstock achieves a compression ratio greater than 1.5:1, on a volume basis.

7. The method of claim 2 wherein the liquor-to-fiber mass ratio of the impregnated material is at most about 3:1.

8. The method of claim 2 wherein the liquor-to-fiber mass ratio of the impregnated material is at most about 2.5:1.

9. The method of claim 2 wherein the impregnating the compressed feedstock comprises adding a surfactant to the feedstock.

10. The method of claim 2 wherein the cooking liquor comprises sodium hydroxide, sodium sulfide, and water.

11. The method of claim 2 wherein the cooking the impregnated material is performed at a cooking temperature between about 150° C. and about 170° C.

12. The method of claim 11 wherein the impregnated material has a residence time of about 30 minutes to about 90 minutes at the cooking temperature.

13. The method of claim 2 wherein the cooking the impregnated material is performed to a kappa number of at most about 35.

14. The method of claim 2 wherein the cooking the impregnated material is performed in a continuous digester.

15. The method of claim 2 further comprising blending the cooked pulp with virgin pulp to yield a pulp blend prior to the bleaching.

16. The method of claim 15 wherein the cooked pulp comprises about 10 percent by weight to about 30 percent by weight of the pulp blend.

17. The method of claim 15 wherein bleaching the cooked pulp comprises bleaching the pulp blend to a GE brightness of at least about 80 percent.

18. A method for manufacturing bleached pulp, the method comprising:

providing a feedstock comprising recycled paper, the recycled paper comprising lignin and cellulose, wherein the feedstock has a solids content of at least 70 percent by weight;

compressing the feedstock having the solids content of at least 70 percent by weight, thereby yielding a compressed feedstock;

impregnating the compressed feedstock having the solids content of at least 70 percent by weight, thereby yielding an impregnated material having a liquor-to-fiber mass ratio of at most about 2.5:1;

feeding the impregnated material having the liquor-to-fiber mass ratio of at most about 2.5:1 to a digester;

cooking the impregnated material having the liquor-to-fiber mass ratio of at most about 2.5:1 to remove at least a portion of the lignin from the impregnated material, thereby yielding a cooked pulp; and

bleaching the cooked pulp.

19. The method of claim 18 wherein the feedstock has a solids content of at least 75 percent by weight.

20. The method of claim 18 wherein the feedstock has a solids content of at least 80 percent by weight.

Continuity (2)
Provisional Application 62958886 · Jan 9, 2020
Related Publication 20230073443A1 · Mar 9, 2023
References Cited (17)
US 3963560A · Mestetsky · 1976 [cited by examiner]
US 5147503A · Nguyen · 1992 [cited by examiner]
US 6017415A · Phillips · 2000 [cited by examiner]
US 11486094B2 · Sixta · 2022 [cited by examiner]
US 20040256065A1 · Aziz et al. · 2004 [cited by applicant]
US 20110120663A1 · Johan et al. · 2011 [cited by applicant]
US 20150225901A1 · Asikainen · 2015 [cited by examiner]
EP 0566284A2 · 1993 [cited by applicant]
EP 0967320A1 · 1999 [cited by applicant]
WO 1997032075A1 · 1997 [cited by applicant]
WO 199907935A1 · 1999 [cited by applicant]
WO 200052256A1 · 2000 [cited by applicant]
WO WO0175220A1 · 2001 [cited by examiner]
WO 2016145276A1 · 2016 [cited by applicant]
WO 2017203329A1 · 2017 [cited by applicant]
Chaz Miller, Profiles in Garbage: Corrugated Boxes, 2001 [downloaded online Apr. 15, 2024], Waste 360. (Year: 2001). [cited by examiner]
ISRI scrap Circular, 208, ISRI. (Year: 2018). [cited by examiner]