IP Library › Granted Patent US 12,353,041
Granted Patent B2
US 12,353,041 · App. 18/109,440 · Granted Jul 8, 2025

Intermittently bonded ribbon with intermittent bonds created with a wet-on-wet process

Inventors: Julie Ann Chalk (Hickory, NC); David Wesley Chiasson (Edmonton, CA); Klaus Hartkorn (Painted Post, NY); Gregory Alan Mills (Clemmons, NC); Xiaomin Zhao (Hickory, NC)
Assignee: CORNING RESEARCH & DEVELOPMENT CORPORATION
G02B6/448
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 12,353,041
App. No.
18/109,440
Granted
Jul 8, 2025
Kind
B2
Abstract

Embodiments of the disclosure relate to an optical fiber ribbon. The optical fiber ribbon includes a plurality of subunits each comprising a subunit coating surrounding at least two optical fibers arranged adjacently to each other. The subunit coating is made of a first material. A plurality of bonds are intermittently formed between adjacent subunits of the plurality of subunits. The plurality of bonds are made of a second material. The optical fiber ribbon includes a diffusion zone at an interface between each of the plurality of bonds and the subunit coating of each adjacent subunit. Each diffusion zone has a gradient of the second material in the first material. Further, the intermittent bonds may include one or more saddle surfaces formed by intersecting convex and concave curvatures. A method of forming such optical fiber ribbons is also disclosed.

Claims (33)

1. An optical fiber ribbon, comprising:

a plurality of subunits each comprising a subunit coating surrounding at least two optical fibers arranged adjacently to each other, the subunit coating comprising a first material;

a plurality of bonds intermittently formed between adjacent subunits of the plurality of subunits, the plurality of bonds comprising a second material; and

a diffusion zone at an interface between each of the plurality of bonds and the subunit coating of each adjacent subunit;

wherein each diffusion zone comprises a gradient of the second material in the first material.

2. The optical fiber ribbon of claim 1 , wherein each diffusion zone has as thickness of 2 μm to 50 μm.

3. The optical fiber ribbon of claim 1 , wherein the second material comprises at least one of a Young's modulus from 25 MPa to 1300 MPa, an elongation at break from 100% to 200%, a specific gravity of 0.9 to 1.2, a tensile strength of 10 MPa to 40 MPa, a viscosity in the range from 100 cP to 8000 cP at 25° C., or a glass transition temperature of 20° C. to 100° C.

4. The optical fiber ribbon of claim 1 , wherein the first material comprises at least one of a Young's modulus of 25 MPa to 1300 MPa, an elongation at break of 10% to 200%, a specific gravity of 0.9 to 1.2, a tensile strength of 10 MPa to 40 MPa, a viscosity in the range from 100 cP to 8000 cP at 25° C., or a glass transition temperature of 30° C. to 100° C.

5. The optical fiber ribbon of claim 1 , wherein the first material is miscible in the second material.

6. The optical fiber ribbon of claim 1 , wherein each of the plurality of bonds comprises at least one saddle surface.

7. The optical fiber ribbon of claim 6 , wherein each bond comprises a first end, a second end, and a central region disposed between the first end and the second end and wherein the at least one saddle surface comprises a first saddle surface located at the first end of the bond.

8. The optical fiber ribbon of claim 7 , wherein the subunit coating is drawn into the first saddle surface.

9. The optical fiber ribbon of claim 7 , wherein the at least one saddle surface comprises a second saddle surface located at the second end of the bond or at the central region of the bond.

10. The optical fiber ribbon of claim 1 , wherein each of the plurality of bonds breaks at a force of 0.2 gf to 75 gf as measured according to a T-peel test.

11. A method of preparing an optical fiber ribbon, comprising:

arranging a plurality of optical fibers adjacent to each other along a length of the optical fiber ribbon;

applying a coating comprising a first material around sets of at least two optical fibers to create a plurality of subunits;

intermittently applying bonds comprising a second material between adjacent subunits of the plurality of subunits, wherein the second material diffuses into the first material creating a diffusion zone of the second material in the first material;

curing the first material and the second material.

12. The method of claim 11 , wherein the step of intermittently applying bonds further comprises depositing droplets of the second material between the adjacent subunits of the plurality of subunits.

13. The method of claim 11 , wherein the second material is miscible in the first material.

14. The method of claim 11 , wherein the diffusion zone has a thickness of 2 μm to 50 μm.

15. The method of claim 11 , wherein the first material comprises a first property and the second material comprises a second property and wherein the diffusion zone comprises a gradient between the first property and the second property.

16. The method of claim 15 , wherein the first property and the second property each comprise at least one of color, Young's modulus, surface friction, ultimate tear strength, or elongation at break.

17. The method of claim 11 , wherein the bonds each comprise at least one saddle surface and wherein the step of intermittently applying the bonds draws the first material of the coating into the saddle surface.

18. An optical fiber ribbon, comprising:

a plurality of subunits each comprising a subunit coating surrounding at least two optical fibers arranged adjacently to each other along a longitudinal axis of the optical fiber ribbon; and

a plurality of bonds intermittently formed between adjacent subunits of the plurality of subunits;

wherein each bond of the plurality of bonds comprises a first end, a second end, and a central region positioned along the longitudinal axis between the first end and the second end;

wherein at least one of the first end, the second end, or the central region of each bond comprises at least one saddle surface comprising intersecting convex and concave curvatures, and

wherein the subunit coating comprises a first material, wherein each bond of the plurality of bonds comprises a second material, and wherein the optical fiber ribbon further comprises a diffusion zone at an interface between each bond of the plurality of bonds and the subunit coating of the adjacent subunits of the plurality of subunits between which the bond is formed, the diffusion zone comprising a gradient of the second material in the first material.

19. The optical fiber ribbon of claim 18 , wherein the diffusion zone has as thickness of 2 μm to 50 μm.

20. The optical fiber ribbon of claim 18 , wherein a first bond in the bonds exhibits cohesive failure when subjected to a force of 0.2 gf to 75 gf as measured according to a T-peel test.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Apr 25, 2023
From: CHALK, JULIE ANN; CHIASSON, DAVID WESLEY; HARTKORN, KLAUS; MILLS, GREGORY ALAN; ZHAO, XIAOMIN
To: CORNING RESEARCH & DEVELOPMENT CORPORATION
Reel/Frame 063426/0238 →
Continuity (3)
Continuation PCTUS2021047260 · Aug 24, 2021
Provisional Application 63072429 · Aug 31, 2020
Related Publication 20230185047A1 · Jun 15, 2023
References Cited (28)
US 5289967A · Bampton et al. · 1994 [cited by applicant]
US 9086555B2 · Namazue et al. · 2015 [cited by applicant]
US 9389386B2 · Matsuzawa et al. · 2016 [cited by applicant]
US 9541722B2 · Sajima et al. · 2017 [cited by applicant]
US 9739965B2 · Isaji et al. · 2017 [cited by applicant]
US 9766397B2 · Homma · 2017 [cited by applicant]
US 9880368B2 · Debban et al. · 2018 [cited by applicant]
US 9995896B2 · Namazue et al. · 2018 [cited by applicant]
US 10007078B2 · Sato et al. · 2018 [cited by applicant]
US 10488609B2 · Sato et al. · 2019 [cited by applicant]
US 20020081084A1 · Matsumoto et al. · 2002 [cited by applicant]
US 20050058409A1 · Miao et al. · 2005 [cited by applicant]
US 20130156390A1 · Matsuzawa et al. · 2013 [cited by applicant]
US 20170031107A1 · Bringuier et al. · 2017 [cited by applicant]
US 20170090135A1 · Sato et al. · 2017 [cited by applicant]
US 20170219790A1 · Debban et al. · 2017 [cited by applicant]
US 20190022962A1 · Moriya et al. · 2019 [cited by applicant]
US 20190204519A1 · Sato et al. · 2019 [cited by applicant]
US 20190250347A1 · Fallahmohammadi et al. · 2019 [cited by applicant]
US 20190317289A1 · Sekine et al. · 2019 [cited by applicant]
US 20200081210A1 · Cignarale et al. · 2020 [cited by applicant]
US 20200271879A1 · Fallahmohammadi et al. · 2020 [cited by applicant]
US 20200292771A1 · Sekine et al. · 2020 [cited by applicant]
US 20220075134A1 · Sato · 2022 [cited by examiner]
WO 2022046710A1 · 2022 [cited by applicant]
European Patent Application No. 21862531.7 Extended European Search Report dated Sep. 3, 2024; 5 Pages; European Patent Office. [cited by applicant]
International Search Report and Written Opinion of the International Searching Authority; PCT/US2021/047260; dated Nov. 30, 2021; 16 pages; United States Patent Office. [cited by applicant]
International Search Report and Written Opinion of the International Searching Authority; PCT/US2021/053322; dated Jan. 11, 2022; pp. 13; International Searching Authority. [cited by applicant]