Apparatus and method for exfoliating graphite
An apparatus and method to exfoliate a graphite grain is described. A mixture of a graphite grain and an ice grain are transferred into a vessel. The vessel includes an agitator. The agitator agitates the mixture to induce a contact between the graphite grain and the ice grain. The contact between the graphite grain and the ice grain exfoliates the graphite grain.
1. A method to exfoliate a graphite grain, the method comprising:
transferring a mixture into a vessel,
wherein the mixture comprises a graphite grain and deionized water,
chilling the deionized water to partially solidify the deionized water to a crystalline structure which adheres to an outer layer of the graphite grain; and
agitating the mixture to induce a contact between the graphite grain and the crystalline structure to exfoliate the outer layer from the graphite grain, wherein the mixture is agitated in a fluid medium, and wherein the fluid medium comprises a first fluid comprising a liquid, wherein the fluid medium comprises a second fluid, and
wherein the second fluid comprises at least one of ethylene glycol, n-methyl-2-pyrrolidone, isopropyl alcohol, methyl alcohol, butyl alcohol, or ethyl alcohol.
2. The method of claim 1 , wherein the agitating comprises agitating the mixture using a rotor.
3. The method of claim 2 , wherein the rotor comprises a first blade.
4. The method of claim 3 , wherein the rotor further comprises a second blade.
5. The method of claim 1 , wherein the agitating comprises agitating the mixture using a vibrator.
6. The method of claim 1 , wherein the second fluid further comprises at least one of air, nitrogen, argon, oxygen, or carbon dioxide.
7. The method of claim 6 , wherein the liquid comprises water.
8. The method of claim 1 , wherein the fluid medium further comprises a surfactant.
9. The method of claim 8 , wherein the surfactant comprises at least one of a soap, an alkyl sulfate, an alkylbenzene sulfonate, a lignosulfonate, or sodium cholate.
10. The method of claim 1 , wherein the crystalline structure comprises ice grains.
11. The method of claim 10 , wherein the ice grains adhere to the graphite grains.
12. The method of claim 11 , further comprising:
melting at least some of the ice grains within the fluid medium.
13. The method of claim 1 , wherein chilling the deionized water to partially solidify the deionized water to a crystalline structure further comprises chilling the deionized water to a temperature sufficient to cause a portion of the deionized water to solidify into the crystalline structure while maintaining another portion of the deionized water in a liquid phase.
14. The method of claim 1 , wherein the mixture is agitated while the fluid medium remains at least partially in the liquid phase during exfoliation of the graphite grain.
15. The method of claim 1 , wherein exfoliation of the outer layer of the graphite grain is in response to contact between the crystalline structure adhered to the graphite grain and the fluid medium during agitation.