Method for debonding temporarily adhesive-bonded carrier-workpiece pair by using chemical and mechanical means

Inventor: Chunbin Zhang (Fremont, CA)
Assignee: DIDREW TECHNOLOGY (BVI) LIMITED
B32B38/10B32B43/006C09J5/00C09J7/201H01L21/6715H01L21/6835H01L21/6836H01L21/7813B32B43/003B32B2457/14C09J2203/326C09J2301/502H01L21/67092H01L2221/6834H01L2221/68318H01L2221/68327H01L2221/68381Y10S156/93Y10S156/941Y10T156/1111Y10T156/1184Y10T156/1967
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,913,254
App. No.
15/916,263
Granted
Feb 9, 2021
Kind
B2
Abstract

In debonding a temporarily adhesive-bonded carrier-workpiece pair by a combination of chemical and mechanical methods, solvents or chemicals are used to remove the adhesives primarily through dissolution, and a thin wire, filament, or blade is used to exert a cutting or wedging action between the carrier and workpiece. The two methods are used together during the debonding process. In the carrier-workpiece pair, the workpiece can be a semiconductor wafer that has been thinned and processed. The carrier and the workpiece are temporarily bonded using an adhesive dissolvable in a selected chemical or solvent. The chemical and mechanical debonding (CMDB) method can be carried out in solvent immersion or in solvent spray to provide high throughput debonding. The dissolved adhesives can be recycled and later reused, thus lowering the cost of the whole bonding and debonding process.

Claims (41)

1. A debonding method comprising:

exposing a carrier-workpiece pair comprising a carrier, a workpiece and an adhesive bonding the carrier and the workpiece, to a chemical solvent selected to dissolve the adhesive, wherein exposing the carrier-workpiece pair to the chemical solvent comprises immersing the carrier-workpiece pair in the chemical solvent to engage the chemical solvent with an exposed edge of the adhesive to dissolve the exposed edge of the adhesive; and

simultaneously with the engagement of the chemical solvent with the exposed edge of the adhesive to dissolve the exposed edge of the adhesive, engaging a wire with the exposed edge of the adhesive and moving the wire relative to the exposed edge of the adhesive to generate turbulent flow action to increase dissolution rate of the chemical solvent.

2. The debonding method of claim 1 ,

wherein moving the wire relative to the exposed edge of the adhesive to generate turbulent flow action to increase dissolution rate of the chemical solvent comprises moving at least one of the wire and the carrier-workpiece pair in a reciprocating saw motion.

3. The debonding method of claim 1 ,

wherein the adhesive comprises a thermoplastic polymer adhesive.

4. The debonding method of claim 1 ,

wherein the workpiece comprises at least one of a semiconductor wafer, an optical lens, quartz, a sapphire wafer, display glass, a liquid crystal display, a thin metal plate, a thin membrane, and a film.

5. The debonding method of claim 1 ,

wherein the workpiece has a thickness of less than 100 microns.

6. The debonding method of claim 1 ,

wherein the wire has a profile of a triangular, polygonal, circular, oval, rectangular, or square shape in cross-section transverse a length thereof.

7. The debonding method of claim 1 ,

wherein the wire has a profile of a saw tooth shape in cross-section along a length thereof.

8. The debonding method of claim 1 , wherein the wire has a profile of a saw tooth shape in cross-section along a length thereof.

9. A debonding method comprising:

spraying a carrier-workpiece pair comprising a carrier, a workpiece and an adhesive bonding the carrier and the workpiece, with a lubricant to engage the lubricant with an exposed edge of the adhesive; and

simultaneously with the engagement of the lubricant with the exposed edge of the adhesive, engaging a wire with the exposed edge of the adhesive and moving the wire relative to the exposed edge of the adhesive to remove parts of the adhesive from the carrier-workpiece pair and allow the lubricant to carry the parts of the adhesive removed and to cool the carrier and the workpiece as the carrier-workpiece is being debonded.

10. The debonding method of claim 9 ,

wherein the workpiece has a thickness of less than 100 microns.

11. The debonding method of claim 10 ,

wherein workpiece comprises a device wafer.

12. The debonding method of claim 9 , wherein the wire has a profile of a triangular, polygonal, circular, oval, rectangular, or square shape in cross-section transverse a length thereof.

13. The debonding method of claim 9 ,

wherein the wire has a profile of a saw tooth shape in cross-section along a length thereof.

14. The debonding method of claim 9 ,

wherein moving the wire relative to the exposed edge of the adhesive comprises moving at least one of the wire and the carrier-workpiece pair in a reciprocating saw motion.

15. The debonding method of claim 9 ,

wherein the adhesive comprises a thermoplastic polymer adhesive.

16. The debonding method of claim 9 ,

wherein the workpiece comprises at least one of a semiconductor wafer, an optical lens, quartz, a sapphire wafer, display glass, a liquid crystal display, a thin metal plate, a thin membrane, and a film.

17. The debonding method of claim 9 ,

wherein the lubricant comprises at least one of water, glycerin and mineral oil.

18. A debonding method comprising:

exposing a carrier-workpiece pair comprising a carrier, a workpiece and an adhesive bonding the carrier and the workpiece, to a chemical solvent selected to dissolve the adhesive, wherein exposing the carrier-workpiece pair to the chemical solvent comprises continuously spraying the chemical solvent on the carrier-workpiece pair to engage the chemical solvent with the exposed edge of the adhesive to dissolve the exposed edge of the adhesive; and

simultaneously with the engagement of the chemical solvent with the exposed edge of the adhesive to dissolve the exposed edge of the adhesive, engaging a wire with the exposed edge of the adhesive and moving the wire relative to the exposed edge of the adhesive to generate turbulent flow action to increase dissolution rate of the chemical solvent.

19. The debonding method of claim 18 ,

wherein moving the wire relative to the exposed edge of the adhesive to generate turbulent flow action to increase dissolution rate of the chemical solvent comprises moving at least one of the wire and the carrier-workpiece pair in a reciprocating saw motion.

20. The debonding method of claim 18 ,

wherein the wire has a profile of a triangular, polygonal, circular, oval, rectangular, or square shape in cross-section transverse a length thereof.

Assignments (6)
CORRECTIVE ASSIGNMENT TO CORRECT THE CONVEYING AND RECEIVING PARTY DATA PREVIOUSLY RECORDED AT REEL: 67676 FRAME: 579. ASSIGNOR(S) HEREBY CONFIRMS THE LICENSE. Recorded Apr 21, 2025
From: DIDREW TECHNOLOGY (BVI) LIMITED
To: ZHANG, CHUNBIN
Reel/Frame 070903/0347 →
LICENSE Recorded Jun 10, 2024
From: ZHANG, CHUNBIN
To: DIDREW TECHNOLOGY (BVI) LIMITED
Reel/Frame 067676/0579 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Nov 4, 2022
From: CHENGDU ESWIN SIP TECHNOLOGY CO., LTD.
To: CHENGDU ESWIN SYSTEM IC CO., LTD.
Reel/Frame 061658/0715 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Feb 16, 2022
From: DIDREW TECHNOLOGY (BVI) LIMITED
To: CHENGDU ESWIN SIP TECHNOLOGY CO., LTD.
Reel/Frame 059168/0448 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jan 27, 2022
From: DIDREW TECHNOLOGY (BVI) LIMITED
To: CHENGDU ESWIN SIP TECHNOLOGY CO., LTD.
Reel/Frame 058795/0321 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Apr 18, 2018
From: ZHANG, CHUNBIN
To: DIDREW TECHNOLOGY (BVI) LIMITED
Reel/Frame 045580/0321 →
Continuity (2)
Provisional Application 62601196 · Mar 15, 2017
Related Publication 20180264797A1 · Sep 20, 2018