IP Library › Granted Patent US 12,318,299
Granted Patent B2
US 12,318,299 · App. 17/179,827 · Granted Jun 3, 2025

Coated implant and method of making the same

Inventors: Oscar A. Quintana-Ponce (Goshen, IN); Bryan J. Smith (Fort Wayne, IN); Craig N. Ernsberger (Granger, IN)
Assignee: DEPUY SYNTHES PRODUCTS, INC.
A61F2/3859A61F2/389A61F2002/30011A61F2002/3863A61F2310/00023A61F2310/00089A61F2310/00095A61F2310/00131A61F2310/00149A61F2310/00892
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 12,318,299
App. No.
17/179,827
Granted
Jun 3, 2025
Kind
B2
Abstract

An orthopaedic knee implant includes a femoral component having a substrate and a coating disposed on the surface of the substrate. A method for making a femoral component of an orthopaedic knee implant is also disclosed.

Claims (37)

1. An orthopaedic knee implant comprising:

a femoral component configured to be coupled to a distal end of a patient's femur, the femoral component comprising

(i) a substrate comprising a titanium alloy having (a) a condylar surface that is curved in a sagittal plane and (b) a bone-facing surface positioned opposite the condylar surface; and

(ii) a coating disposed on the condylar surface, the coating comprising (a) a bonding layer comprising niobium, zirconium, titanium, tantalum, platinum, molybdenum, an alloy thereof, or combinations thereof, (b) an outer ceramic layer, and (c) a second layer comprising a plurality of alternating sublayers positioned between and interconnecting the bonding layer and the outer ceramic layer, wherein at least one sublayer of the second layer has a thickness of about 5 nm to about 500 nm, and wherein at least one sublayer of the second layer comprises at least about 95% niobium nitride,

wherein (i) the plurality of alternating sublayers are configured to resist crack propagation from the outer ceramic layer, the plurality of alternating sublayers include a number of metallic sublayers and a number of ceramic sublayers that are harder than the metallic sublayers, and (ii) the outer ceramic layer forms an outer articular surface of the femoral component and is shaped to contact a concave proximal surface of a tibial bearing.

2. The implant of claim 1 , wherein the second layer comprises at least eight sublayers, wherein the sublayers comprise alternating zirconium nitride and niobium nitride sublayers.

3. The implant of claim 2 , wherein each zirconium nitride sublayer of the alternating sublayers has a thickness of about 5 nm to about 200 nm.

4. The implant of claim 3 , wherein the second layer has a thickness of about 3 μm to about 8 μm.

5. The implant of claim 1 , wherein the outer ceramic layer comprises at least about 90% monoclinic oxidized zirconium.

6. The implant of claim 5 , wherein the outer ceramic layer has a thickness of about 100 nm to about 5 μm.

7. The implant of claim 6 , wherein at least one sublayer of the second layer comprises at least about 95% zirconium nitride.

8. The implant of claim 1 , wherein the bonding layer comprises at least about 90% zirconium.

9. The implant of claim 8 , wherein the bonding layer has a thickness of about 50 nm to about 2 μm.

10. The implant of claim 1 , wherein the femoral component comprises a bone-engaging layer disposed on the bone-facing surface.

11. The implant of claim 10 , wherein the bone-engaging layer is porous.

12. The implant of claim 1 , wherein the second layer comprises an inner sublayer and an outer sublayer.

13. The implant of claim 12 , wherein the inner sublayer and the outer sublayer have the same composition.

14. The implant of claim 12 , wherein the second layer comprises an intermediate sublayer having a composition different from the inner sublayer, the outer sublayer, or both.

15. A process for forming a femoral component of an orthopaedic knee implant, the process comprising:

depositing a first layer comprising niobium, zirconium, titanium, tantalum, platinum, molybdenum, or combinations thereof on a condylar surface of a substrate comprising titanium, wherein the condylar surface is curved in a sagittal plane; and

depositing one or more alternating sublayers to form a second layer,

wherein depositing the alternating sublayers to form the second layer comprises:

(a) creating a sublayer of zirconium nitride on the first layer,

(b) creating a sublayer of niobium on the sublayer of zirconium nitride, and

(c) repeating steps (a) and (b) to form the second layer.

16. The process of claim 15 , comprising oxidizing a portion of the second layer to form a third layer comprising oxidized zirconium.

17. The process of claim 15 , comprising depositing a third layer on an outer surface of the second layer.

18. The process of claim 17 , wherein the third layer comprises zirconium oxide, niobium oxide, zirconium oxynitride, niobium oxynitride, or a combination thereof.

19. An orthopaedic knee implant comprising:

a femoral component configured to be coupled to a distal end of a patient's femur, the femoral component comprising

(i) a substrate comprising a titanium alloy having (a) a condylar surface that is curved in a sagittal plane and (b) a bone-facing surface positioned opposite the condylar surface; and

(ii) a coating disposed on the condylar surface, the coating comprising (a) a bonding layer comprising niobium, zirconium, titanium, tantalum, platinum, molybdenum, an alloy thereof, or combinations thereof, (b) an outer ceramic layer, and (c) a second layer comprising a plurality of alternating sublayers positioned between and interconnecting the bonding layer and the outer ceramic layer, wherein the second layer comprises an inner sublayer and an outer sublayer, and wherein the second layer comprises an intermediate sublayer having a composition different from the inner sublayer, the outer sublayer, or both,

wherein (i) the plurality of alternating sublayers are configured to resist crack propagation from the outer ceramic layer, the plurality of alternating sublayers include a number of metallic sublayers and a number of ceramic sublayers that are harder than the metallic sublayers, and (ii) the outer ceramic layer forms an outer articular surface of the femoral component and is shaped to contact a concave proximal surface of a tibial bearing.

20. The implant of claim 19 , wherein the second layer comprises at least eight sublayers of alternating zirconium nitride and niobium nitride sublayers.

21. The implant of claim 19 , wherein the outer ceramic layer comprises at least about 90% monoclinic oxidized zirconium.

22. The implant of claim 19 , wherein at least one sublayer of the second layer has a thickness of about 5 nm to about 500 nm.

23. The implant of claim 19 , wherein the bonding layer comprises at least about 90% zirconium.

Assignments (2)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded May 6, 2025
From: QUINTANA-PONCE, OSCAR A.; SMITH, BRYAN J.; ERNSBERGER, CRAIG N.
To: DEPUY SYNTHES PRODUCTS, INC.
Reel/Frame 071038/0776 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Aug 12, 2021
From: QUINTANA-PONCE, OSCAR A.; SMITH, BRYAN J.; ERNSBERGER, CRAIG N.
To: DEPUY SYNTHES PRODUCTS, INC.
Reel/Frame 057160/0061 →
Continuity (4)
Provisional Application 63010300 · Apr 15, 2020
Provisional Application 62978534 · Feb 19, 2020
Provisional Application 62978537 · Feb 19, 2020
Related Publication 20210251766A1 · Aug 19, 2021
References Cited (41)
US 3643658A · Steinemenan · 1972 [cited by applicant]
US 5037438A · Davidson · 1991 [cited by applicant]
US 5169597A · Davidson et al. · 1992 [cited by applicant]
US 5370694A · Davidson · 1994 [cited by applicant]
US 5980974A · Armini et al. · 1999 [cited by applicant]
US 7157096B2 · Zhang et al. · 2007 [cited by applicant]
US 7393589B2 · Aharonov · 2008 [cited by applicant]
US 7790216B2 · Popoola et al. · 2010 [cited by applicant]
US 8147560B2 · Zeller · 2012 [cited by examiner]
US 8187620B2 · Chandrasekaran et al. · 2012 [cited by applicant]
US 8790345B2 · Anderson · 2014 [cited by applicant]
US 9005769B2 · Lambert · 2015 [cited by applicant]
US 9404173B2 · Walker · 2016 [cited by applicant]
US 10272177B2 · Khowaylo · 2019 [cited by applicant]
US 10543297B2 · Pawar · 2020 [cited by applicant]
US 20040002766A1 · Hunter · 2004 [cited by examiner]
US 20040122524A1 · Hunter et al. · 2004 [cited by applicant]
US 20080255674A1 · Rahaman · 2008 [cited by examiner]
US 20090054985A1 · Anderson · 2009 [cited by applicant]
US 20090125115A1 · Popoola · 2009 [cited by examiner]
US 20090187255A1 · Jani et al. · 2009 [cited by applicant]
US 20110066253A1 · Langhorn et al. · 2011 [cited by applicant]
US 20110112651A1 · Blaylock · 2011 [cited by examiner]
US 20120035739A1 · Wilhemsson et al. · 2012 [cited by applicant]
US 20130216420A1 · Li et al. · 2013 [cited by applicant]
US 20130230640A1 · Pawar · 2013 [cited by examiner]
CN 101596607A · 2009 [cited by applicant]
CN 102181835A · 2011 [cited by applicant]
CN 102277554A · 2011 [cited by applicant]
JP 2006511272A · 2006 [cited by applicant]
JP 2012110704A · 2012 [cited by applicant]
Cui, Wenfang et al., “Bio-tribocorrosion behavior of nanocrystalline TiZrN coating on biomedical titanium alloy,” Surface & Coatings Technology 369 (2019) 79-86. [cited by applicant]
Donohue, L.A. et al., “Deposition and characterization of arc-bond sputter Ti [cited by applicant]
Huang, Jia-Hong et al., “Evaluation of the fracture toughness of Ti [cited by applicant]
Huang, Jia-Hong et al., “Oxidation behavior and corrosion resistance of vacuum annealed ZrN-coated stainless steel,” Surface & Coatings Technology 358 (2019) 308-319. [cited by applicant]
Huang, Jia-Hong et al., “Phase transition and mechanical properties of ZrN [cited by applicant]
Lin, Yu-Wei et al., “Effect of Ti interlayer thickness on mechanical properties and wear resistance of TiZrN coatings on AlSl D2 steel,” Surface & Coatings Technology 394 (2020) 125690. [cited by applicant]
Milošev, I. et al., “Comparison of TiN, ZrN and CrN hard nitride coatings: Electrochemical and thermal oxidation,” Thin Solid Films 303 (1997) 246-254. [cited by applicant]
Qi, Z.B. et al., “In situ and ex situ studies of microstructure evolution during high-temperature oxidation of ZrN hard coating,” Scripta Materialia 97 (2015) 9-12. [cited by applicant]
Patent Cooperation Treaty Invitation to Pay Fees for corresponding International Application No. PCT/IB2021/051430, dated May 12, 2021, 14 pages. [cited by applicant]
Advanced Surface Technology Why Take a Chance With Anything Else, Aesculap Implant Systems, 2017, 12 pages. [cited by applicant]