IP Library Granted Patent US 12,668,041
Granted Patent B2
US 12,668,041 · App. 18/152,807 · Granted Jun 30, 2026

Protective display film with glass

Inventors: Joseph W. Woody, V (Woodbury, MN); David Scott Thompson (Bayport, MN); Catherine A. Leatherdale (Woodbury, MN); Ryan M. Braun (St. Paul, MN); Michael A. Johnson (Stillwater, MN); Steven D. Solomonson (Shoreview, MN); John J. Stradinger (Roseville, MN); Lyudmila A. Pekurovsky (Bloomington, MN); Joseph D. Rule (Woodbury, MN); Peter D. Condo (Lake Elmo, MN)
Assignee: 3M Innovative Properties Company
B32B17/06B32B7/12B32B27/308B32B27/40H10K59/873H10K77/111B32B2307/56B32B2315/08B32B2333/04B32B2375/00B32B2457/206H10K2102/311
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 12,668,041
App. No.
18/152,807
Granted
Jun 30, 2026
Kind
B2
Abstract

A display film includes a transparent glass layer having a thickness of 250 micrometers or less, or in a range from 25 to 100 micrometers. A transparent energy dissipation layer is fixed to the transparent glass layer. The transparent energy dissipation layer has a glass transition temperature of 27 degrees Celsius or less and a Tan Delta peak value of 0.5 or greater, or from 1 to 2.

Claims (31)

1 . A display film comprising:

a transparent glass layer having a thickness of 250 micrometers or less; and

a transparent energy dissipation layer fixed to the transparent glass layer, the transparent energy dissipation layer comprising a cross-linked polyurethane and having a glass transition temperature 27 degrees Celsius and negative 25 degrees Celsius and a Tan Delta peak value between 0.5 and 2.0,

wherein the display film has a haze of 2.0% or less.

2 . The display film according to claim 1 , wherein the transparent energy dissipation layer comprises a cross-linked polyurethane acrylate layer.

3 . The display film according to claim 1 , wherein the transparent energy dissipation layer has a glass transition temperature 10 degrees Celsius and negative 25 degrees Celsius.

4 . The display film according to claim 1 , wherein the transparent energy dissipation layer has a thickness in a range from 20 to 200 micrometers.

5 . The display film according to claim 1 , wherein the transparent energy dissipation layer is directly fixed to the transparent glass layer.

6 . The display film according to claim 1 , wherein the transparent energy dissipation layer is fixed to the transparent glass layer by an intermediate adhesive layer.

7 . The display film according to claim 1 , further comprising a protective layer fixed to the transparent glass layer, and the transparent glass layer separates the transparent energy dissipation layer from the protective layer.

8 . The display film according to claim 7 , further comprising an optically clear adhesive layer separating the protective layer from the transparent glass layer.

9 . The display film according to claim 1 , further comprising a coupling layer disposed on the transparent energy dissipation layer, and the transparent energy dissipation layer separates the coupling layer from the transparent glass layer, the coupling layer having a shear modulus of 200 kPa or less over a temperature range from −40 degrees Celsius to 70 degrees Celsius.

10 . The display film according to claim 9 , further comprising a release liner contacting the coupling layer.

11 . The display film according to claim 1 , wherein the transparent energy dissipation layer has a Tan Delta peak value of 0.5 or greater, and the transparent energy dissipation layer has a cross-link density in a range from 0.1 to 1.0 mol/kg.

12 . The display film according to claim 1 , wherein the display film has a visible light transmission of 85% or greater.

13 . The display film according to claim 1 , wherein the display film has a thickness in a range from 30 to 300 micrometers.

14 . A display film comprising:

a transparent glass layer having a thickness of 250 micrometers or less;

a transparent energy dissipation layer fixed to the transparent glass layer, the transparent energy dissipation layer comprising a cross-linked polyurethane and having glass transition temperature 27 degrees Celsius and negative 25 degrees Celsius and a Tan Delta peak value between 0.5 and 2.0; and

a protective layer fixed to the transparent glass layer, the transparent glass layer separates the transparent energy dissipation layer from the protective layer,

wherein the display film has a haze of 2.0% or less.

15 . The display film according to claim 14 , further comprising a coupling layer disposed on the transparent energy dissipation layer, the transparent energy dissipation layer separates the coupling layer from the transparent glass layer.

16 . The display film according to claim 15 , further comprising a release liner contacting the coupling layer.

17 . A display film comprising:

a transparent glass layer having a thickness of 250 micrometers or less;

a transparent energy dissipation layer fixed to the transparent glass layer, the transparent energy dissipation layer comprising a crosslinked polyurethane and has a glass transition temperature 27 degrees Celsius and negative 25 degrees Celsius, a Tan Delta peak value between 0.5 and 2.0;

an optically clear adhesive layer disposed on the transparent glass layer; and

a protective layer disposed on the optically clear adhesive layer, and the optically clear adhesive layer separates the transparent energy dissipation layer from the protective layer,

wherein the display film has a haze of 2.0% or less.

18 . The display film according to claim 17 , further comprising a coupling layer disposed on the transparent energy dissipation layer, the transparent energy dissipation layer separates the coupling layer from the transparent glass layer.

19 . The display film according to claim 18 , further comprising a release liner contacting the coupling layer.

Continuity (3)
Continuation 16335537
Provisional Application 62397584 · Sep 21, 2016
Related Publication 20230158777A1 · May 25, 2023
References Cited (74)
US 3391053A · Kolb · 1968 [cited by applicant]
US 3574030A · Callander et al. · 1971 [cited by applicant]
US 6376590B2 · Kolb et al. · 2002 [cited by applicant]
US 6815070B1 · Bürkle et al. · 2004 [cited by applicant]
US 7241437B2 · Davidson et al. · 2007 [cited by applicant]
US 7980910B2 · Padiyath et al. · 2011 [cited by applicant]
US 10005264B2 · Leatherdale et al. · 2018 [cited by applicant]
US 10662276B2 · Colson et al. · 2020 [cited by applicant]
US 11577492B2 · Woody, V · 2023 [cited by examiner]
US 11631829B2 · Eckert · 2023 [cited by examiner]
US 20030111159A1 · Hashimoto et al. · 2003 [cited by applicant]
US 20040052080A1 · Hieda et al. · 2004 [cited by applicant]
US 20040266900A1 · Neff · 2004 [cited by examiner]
US 20050038133A1 · Neff · 2005 [cited by examiner]
US 20050084622A1 · Houghtaling et al. · 2005 [cited by applicant]
US 20050147813A1 · Gotz et al. · 2005 [cited by applicant]
US 20060148950A1 · Davidson et al. · 2006 [cited by applicant]
US 20070092733A1 · Yang et al. · 2007 [cited by applicant]
US 20080020170A1 · Haubrich et al. · 2008 [cited by applicant]
US 20080220245A1 · Suzuki et al. · 2008 [cited by applicant]
US 20080241524A1 · Fukuda et al. · 2008 [cited by applicant]
US 20090004478A1 · Baetzold et al. · 2009 [cited by applicant]
US 20090105437A1 · Determan et al. · 2009 [cited by applicant]
US 20090280329A1 · Rukavina et al. · 2009 [cited by applicant]
US 20110045306A1 · Johnson et al. · 2011 [cited by applicant]
US 20120229893A1 · Hebrink et al. · 2012 [cited by applicant]
US 20130335823A1 · Epstein et al. · 2013 [cited by applicant]
US 20140370307A1 · Hao et al. · 2014 [cited by applicant]
US 20150266272A1 · Lee et al. · 2015 [cited by applicant]
US 20150325814A1 · Yang et al. · 2015 [cited by applicant]
US 20150330597A2 · Schaffer et al. · 2015 [cited by applicant]
US 20160002103A1 · Wang et al. · 2016 [cited by applicant]
US 20160168432A1 · You et al. · 2016 [cited by applicant]
US 20160185926A1 · Song et al. · 2016 [cited by applicant]
US 20160312363A1 · Yamashita et al. · 2016 [cited by applicant]
US 20160376025A1 · Bimanand · 2016 [cited by examiner]
US 20170100920A1 · Matsumori et al. · 2017 [cited by applicant]
US 20180051123A1 · Rukavina · 2018 [cited by examiner]
US 20180053451A1 · Han · 2018 [cited by examiner]
US 20180315953A1 · Hu et al. · 2018 [cited by applicant]
US 20190140214A1 · Kim et al. · 2019 [cited by applicant]
US 20200309999A1 · Thompson et al. · 2020 [cited by applicant]
US 20210139748A1 · Behling · 2021 [cited by examiner]
US 20230120549A1 · Rukavina · 2023 [cited by examiner]
JP 04117463A · 1992 [cited by applicant]
JP 2002180019A · 2002 [cited by applicant]
JP 2005239977A · 2005 [cited by applicant]
JP 2005288787A · 2005 [cited by applicant]
JP 2010107956A · 2010 [cited by applicant]
JP 2016060833A · 2016 [cited by applicant]
KR 20100023355A · 2010 [cited by applicant]
WO 2003094256A2 · 2003 [cited by applicant]
WO 2009120548A2 · 2009 [cited by applicant]
WO 2009148722A2 · 2009 [cited by applicant]
WO 2011056396A2 · 2011 [cited by applicant]
WO 2012138675A1 · 2012 [cited by applicant]
WO 2014035942A1 · 2014 [cited by applicant]
WO 2014092422A1 · 2014 [cited by applicant]
WO 2014133925A1 · 2014 [cited by applicant]
WO 2014152819A1 · 2014 [cited by applicant]
WO 2014197194A1 · 2014 [cited by applicant]
WO 2014197368A1 · 2014 [cited by applicant]
WO 2015188029A1 · 2015 [cited by applicant]
WO 2015191949A1 · 2015 [cited by applicant]
WO 2016028542A1 · 2016 [cited by applicant]
WO 2016106207A1 · 2016 [cited by applicant]
WO 2017105850A1 · 2017 [cited by applicant]
WO 2017214105A2 · 2017 [cited by applicant]
WO 2018005833A2 · 2018 [cited by applicant]
“Silicone PSAs”, ASI Adhesives & Sealants Industry, PSTC Week of Learning, 2006, URL: <http//www.pstc.org>, pp. 1-12. [cited by applicant]
Charlesby, “Elastic Modulus Formulae For A Crosslinked Network”, International Journal of Radiation Applications And Instrumentation. Part C. Radiation Physics And Chemistry, 1992, vol. 40, No. 02, pp. 117-120. [cited by applicant]
DMA Q800 Specifications, TA Instruments, 2010, pp. 75-96. [cited by applicant]
International Search report for PCT International Application No. PCT/US2017/052770, mailed on Jan. 9, 2018, 6 pages. [cited by applicant]
Pongmuksuwan, “Synthesis and characterization of soft polyurethane for pressure ulcer prevention”, Polymer Testing, 2022, vol. 112, No. 107634, pp. 1-11. [cited by applicant]