Powder composition, coating film, and three-dimensional shaped article
A powder composition containing an aromatic polyetherketone resin (I) and a fluorine-containing copolymer (II). The powder composition has a ratio r2/r1 of 1.60 or lower, wherein r1 represents an average dispersed particle size of the fluorine-containing copolymer (II) and r2 represents an average dispersed particle size of the fluorine-containing copolymer (II) after melt flow rate measurement at 380° C. and a load of 5000 g with 5-minute pre-heating in conformity with ASTM D1238.
1 . A powder composition comprising:
an aromatic polyether ketone resin (I); and
a fluorine-containing copolymer (II),
wherein the powder composition has a ratio r2/r1 of 1.60 or lower, wherein r1 represents an average dispersed particle size of the fluorine-containing copolymer (II) and r2 represents an average dispersed particle size of the fluorine-containing copolymer (II) after melt flow rate measurement at 380° C. and a load of 5000 g with 5-minute pre-heating in conformity with ASTM D1238.
2 . The powder composition according to claim 1 ,
wherein the aromatic polyether ketone resin (I) and the fluorine-containing copolymer (II) have a ratio by mass (I):(II) of 99:1 to 30:70.
3 . The powder composition according to claim 1 ,
wherein the aromatic polyether ketone resin (I) has a melting point of 300° C. to 380° C.
4 . The powder composition according to claim 1 ,
wherein the aromatic polyether ketone resin (I) has a glass transition temperature of 130° C. to 220° C.
5 . The powder composition according to claim 1 ,
wherein the fluorine-containing copolymer (II) has a melting point of 200° C. to 323° C.
6 . The powder composition according to claim 1 , further comprising an additive.
7 . The powder composition according to claim 6 ,
wherein the additive comprises a fibrous filler (III).